EPOXYLITE E6107

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

EPOXYLITE E6107

Main features

  • Equal-Weight Two-Component Mixing
  • Two-Day Room-Temperature Pot Life
  • VPI and Vacuum Impregnation

Product Description

EPOXYLITE E6107 Hi Temp Epoxy Resin System is a two-component heat-cured impregnation and casting system with a viscous liquid resin and fluid liquid hardener. It is used for VPI, vacuum impregnation, and bench casting of motor armatures, stators, coils, and glass-wrapped electrical or structural components. The components mix at 100:100 by weight. Typical resin viscosity is 18,000 to 28,000 cP, while hardener viscosity is 150 to 400 cP. A staged heat cure develops Shore D 90 hardness together with stated mechanical and electrical insulation properties.

Key features

  • Equal-weight component mixing: The resin and hardener use a 100:100 mix ratio by weight.
  • Extended processing window: The mixed system has a pot life of at least two days at room temperature.
  • Impregnation and casting versatility: The system supports VPI, vacuum impregnation, and bench casting processes.

Applications

  • Impregnation of motor armatures, stators, and coils
  • Impregnation and casting of glass-wrapped electrical and structural components
Product Family

EPOXYLITE E6107

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Flash Point
94 °C
Electrical Properties
Dielectric Strength
19 kV/mm
Volume Resistivity
4.2 x 10^16 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component and mixed-system values before heat cure.

Property Value Unit Method / condition
Resin viscosity 18,000 to 28,000 cP As supplied; resin component
Hardener viscosity 150 to 400 cP As supplied; hardener component
Mix ratio by weight 100:100 - Resin:hardener
Pot life at room temperature >= 2 days Mixed system
Pot life at 121 deg C 30 min Mixed system at elevated temperature
Technical properties

After-processing / final-state properties

Typical cured properties apply after the stated staged heat cure.

Property Value Unit Method / condition
Cure schedule 3 h at 121 deg C plus 3 h at 135 deg C - Heat-cured system
Hardness 90 Shore D Typical cured material
Tensile strength 9,800 psi Typical cured material
Flexural strength 17,000 psi Typical cured material
Dielectric strength 480 V/mil At 125 mil specimen thickness
Volume resistivity 4.2 x 10^16 ohm cm Typical cured material