Main features

  • Low-Viscosity Winding Impregnation
  • Fast 30-Minute Heat Cure
  • Hermetic Compressor Insulation

Product Description

EPOXYLITE E6001 Hermetic Epoxy Impregnating Resin is a solvent-borne epoxy insulating varnish for dip-and-bake impregnation of motor windings used in hermetic compressors and refrigeration equipment. The clear amber liquid has 36 to 40% nonvolatile content, typical viscosity of 100 to 200 cP, and a flash point of 13 deg C. stated cure options include two hours at 77 deg C followed by six hours at 135 deg C, or 30 minutes at 177 deg C. The product supports winding impregnation where a low-viscosity epoxy varnish and controlled thermal cure are required.

Key features

  • Low-viscosity winding impregnation: Typical viscosity is 100 to 200 cP in the as-supplied clear amber liquid.
  • Controlled nonvolatile content: The varnish contains 36 to 40% nonvolatile material.
  • Heat-cure flexibility: Documented cure options include a staged 77/135 deg C cycle or 30 minutes at 177 deg C.

Applications

  • Motor-winding impregnation for hermetic compressors
  • Motor-winding impregnation for refrigeration units
  • Dip-and-bake insulating varnish applications
Product Family

EPOXYLITE E6001

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
clear amber liquid
Physical Properties
Viscosity
100-200 mPa.s
Thermal Properties
Flash Point
13 °C
Electrical Properties
Dielectric Strength
157.48 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied values for the solvent-borne epoxy insulating varnish.

Property Value Unit Method / condition
Appearance Clear amber liquid - As supplied
Nonvolatile content 36 to 40 % As supplied
Viscosity 100 to 200 cP As supplied
Weight per gallon 8.2 to 8.5 lb/gal As supplied
Flash point 13 deg C Equivalent to 55 deg F
Volatile organic content 5.2 lb/gal As supplied