EPOXYLITE E234

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

EPOXYLITE E234

Main features

  • Low-Temperature Trickle Impregnation
  • 15-25 Minute Gel Window
  • Class 155 Electrical Insulation

Product Description

EPOXYLITE E234 Two-Component Epoxy Impregnating Resin is a 100% solids, two-component epoxy system for low-temperature trickle impregnation of motor and transformer windings. The E234 resin and C234 hardener mix at 100:20 by weight or 100:22.3 by volume, producing a typical mixed viscosity of 800 to 1,800 cP and a 15 to 25 minute gel time. The cured system is associated with Class 155 electrical insulation and typical dielectric strength of 1,200 volts/mil. Supported uses include high-speed armatures, appliance motors, transformers, and other high-speed rotating equipment.

Key features

  • Low-temperature trickle impregnation: The mixed system is formulated for motor and transformer winding impregnation with a 15 to 25 minute gel time.
  • Controlled component mixing: The documented mix ratio is 100:20 by weight or 100:22.3 by volume.
  • Class 155 electrical insulation: Typical cured data include Shore D 87 and dielectric strength of 1,200 volts/mil.

Applications

  • Trickle impregnation of motor windings
  • Trickle impregnation of transformer windings
  • High-speed armatures
  • Appliance motors and high-speed rotating equipment
Product Family

EPOXYLITE E234

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity
800-1800 mPa.s
Viscosity (Part A)
1000-2000 mPa.s
Thermal Properties
Flash Point
94 °C
Chemical Properties
Water Absorption
0.2 %
Electrical Properties
Dielectric Strength
47.2 kV/mm
Volume Resistivity
8.0 x 10^14 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component and mixed-system values for the E234 resin and C234 hardener before cure.

Property Value Unit Method / condition
Resin viscosity 1,000 to 2,000 cP E234 resin as supplied
Hardener viscosity 100 to 500 cP C234 hardener as supplied
Mix ratio by weight 100:20 - E234 resin:C234 hardener
Mix ratio by volume 100:22.3 - E234 resin:C234 hardener
Mixed viscosity 800 to 1,800 cP Mixed system
Gel time 15 to 25 min Mixed system
Technical properties

After-processing / final-state properties

Typical final-state values for the cured impregnating-resin system.

Property Value Unit Method / condition
Thermal class 155 deg C Electrical insulation classification stated for the system
Post-cure 15 min At 100 deg C
Shore D hardness 87 - Typical cured value
Dielectric strength 1,200 volts/mil Typical cured value
Volume resistivity 8.0 x 10^14 ohm cm Typical cured value

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers