EPOCAST 50-A1/946

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

EPOCAST 50-A1/946

Main features

  • Short 20-Minute Gel Time
  • Solvent-Free Composite Laminating
  • High-Strength Cured Laminate

Product Description

EPOCAST 50-A1 Resin / Hardener 946 Epoxy Laminating System is an unfilled, solvent-free two-component epoxy for composite structure manufacture, repair, and filament winding. The amber system mixes at 100:15 by weight and has a 20-minute gel time at 25 deg C, providing the shorter work-life option in the 50-A1 series. It can be cured for five days at 25 deg C or heat-cured for two hours at 77 to 93 deg C after room-temperature gel. Typical cured glass-laminate data include compressive strength above 46 ksi and self-extinguishing behavior.

Key features

  • Short working window: The mixed system has a 20-minute gel time at 25 deg C.
  • Solvent-free laminating system: The unfilled epoxy is used for composite manufacture, repair, and filament winding.
  • Cured laminate strength: Typical compressive strength exceeds 46 ksi across the reported cure conditions.

Applications

  • Composite structure manufacture
  • Composite repair
  • Filament winding
Product Family

EPOCAST 50-A1/946

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
White
Pot Life
2-5 minutes
Physical Properties
Viscosity (Part A)
7,770 mPa.s
Viscosity (Part B)
400 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
70 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-received values distinguish the resin, hardener, and mixed system.

Property Value Unit Method / condition
Color 50-A1 resin amber; 946 hardener straw; mixed system amber - Visual
Density 50-A1 1.21; 946 1.05; mixed 1.18 g/cm^3 ASTM D792
Viscosity 50-A1 7,770; 946 400; mixed 2,400 cP At 25 deg C; ASTM D2196
Mix ratio by weight 100:15 - 50-A1 resin:Hardener 946
Gel time 20 min 100 g mass at 25 deg C; ASTM D2471
Shelf life 12 months Components unopened at 25 deg C
Technical properties

After-processing / final-state properties

Typical cured laminate properties vary with the stated cure schedule.

Property Value Unit Method / condition
Cure schedule 5 days at 25 deg C; or 2 h at 77 to 93 deg C after room-temperature gel - Typical cure options
Handling and machining 8 to 16 h At room temperature
Compressive strength 46.03; 50.58; 48.30 ksi 7 days at 25 deg C; 27 days at 25 deg C; 1 day at 25 deg C plus 2 h at 66 deg C; ASTM D695
Compressive modulus 4.04; 3.43; 3.66 Msi Same cure sequence as compressive strength; ASTM D695
Self-extinguishing time 0 s 60-second vertical test; 7-day and heat-cured specimens
Burn length < 6 (< 15) in (cm) FAR 25.853A; 60-second vertical test

Leading Brands Trust in Our Products and Services