EPOCAST 169-1

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

EPOCAST 169-1

Main features

  • Low-Density Epoxy Syntactic Resin
  • Paste Consistency for Application
  • Machinable Application Paste Material

Product Description

EPOCAST 169A-1 Resin is the resin component of a general-purpose, low-density epoxy syntactic material. It is supplied as a red-brown paste with a typical density of 0.56 g/cm³ at 25°C. The available resin-specific data emphasize its physical form, appearance, and low-density character for product identification and preparation before processing. This page covers EPOCAST 169A-1 Resin only; mixed-material processing information, qualification statements, storage data presented jointly for both components, and cured-system performance values have been excluded.

Key features

  • Low-density resin: Typical as-supplied density of 0.56 g/cm³.
  • Paste consistency: Supplied as a paste at 25°C.
  • Red-brown appearance: Provides clear visual identification of the resin component.
Product Family

EPOCAST 169-1

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Red-Brown
Density (g)
0.56 g/cm3

Additional Information

Technical properties

As-supplied resin properties

Typical properties of the EPOCAST 169A-1 resin component before mixing or processing.

Property Value Unit Method / condition
Color Red-brown — Visual; resin component
Density 0.56 g/cm³ Typical value; ASTM D1622
Viscosity / consistency Paste — At 25°C; ASTM D2196