EPOCAST 1636

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

EPOCAST 1636

Main features

  • High-Density Casting Material
  • High Temperature Potting Compound
  • Self-Extinguishing Bonding Material

Product Description

EPOCAST 1636-A/B is a two-part, aluminum-filled epoxy syntactic potting compound for high-density and elevated-temperature applications. The medium-viscosity system mixes at 100:8 by weight and cures to a strong, machinable gray material. It is used to reinforce honeycomb structures and is qualified to BMS 5-28, Type 6. Typical cured data include compressive strengths up to 28.0 ksi (193 MPa), and the material is self-extinguishing under BSS-7230-F4. Its extended gel time, alternative room-temperature and heat-cure schedules, mechanical strength, and low measured fluid-immersion weight gain support demanding structural potting and reinforcement work.

Key features

  • High-temperature compressive performance: Delivers a typical compressive strength of 28.0 ksi (193 MPa) when tested at 25°C after 14 days of exposure at 177°C.
  • Controlled two-part processing: Features a 100:8 weight mix ratio, 29,000 cP mixed viscosity, and 120-minute gel time for a 50 g mass at 25°C.
  • Qualified structural reinforcement: Used for honeycomb reinforcement, qualified to BMS 5-28, Type 6, and self-extinguishing under BSS-7230-F4.
Product Family

EPOCAST 1636

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Gray
Density (g)
1.72 g/cm3
Mix Ratio
100:8
Physical Properties
Viscosity
29000 mPa.s
Viscosity (Part A)
38000 mPa.s
Viscosity (Part B)
1000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component and mixed-system properties. Values are provided for product evaluation and are not guaranteed specifications.

Property Value Unit Method / condition
Color Part A: gray; Part B: dark amber; mixed system: gray — Visual
Density Part A: 1.73; Part B: 1.07; mixed system: 1.72 g/cm³ ASTM D792
Viscosity Part A: 38,000; Part B: 1,000; mixed system: 29,000 cP ASTM D2196 at 25°C
Mix ratio 100:8 Parts by weight Part A resin to Part B hardener; mix thoroughly while minimizing air entrapment
Gel time 120 Minutes ASTM D2471; 50 g mixed mass at 25°C
Material temperature before mixing Above 18 °C Equivalent to above 65°F
Cure schedules 7 days at 25°C; 90 minutes at 127°C; or 60 minutes at 177°C — For elevated-temperature cures, gel at 25°C and increase temperature approximately 3–4°C per minute to the target temperature
Shelf life 1 Year Store dry in sealed original containers at 2–40°C and protect from direct sunlight; expiration may vary by customer specification
Technical properties

After-processing / final-state properties

Typical cured properties are provided for product evaluation and are not specification values. Results depend on the stated cure, conditioning, substrate, and test temperature.

Property Value Unit Method / condition
Compressive strength 15.0 (103) ksi (MPa) ASTM D695; cured 7 days at 25°C
Compressive strength 28.0 (193) ksi (MPa) ASTM D695; room-temperature gel followed by 1.5 hours at 121°C
Compressive strength after heat exposure 28.0 (193) ksi (MPa) ASTM D695; tested at 25°C after 14 days at 177°C
Compressive strength at elevated temperature 5.0 (34.5) ksi (MPa) ASTM D695; tested at 177°C after 14 days at 177°C
Compressive modulus 800 (5,517) ksi (MPa) ASTM D695; cured 7 days at 25°C
Tensile lap shear 2,000 (13.8) psi (MPa) ASTM D1002; etched aluminum-to-aluminum specimens
Flammability Self-extinguishing — BSS-7230-F4
Weight gain after immersion <0.1 % ASTM D543; 24 hours at 25°C in TT-S-735 Type III test fluid, MIL-M-5606 hydraulic fluid, Skydrol hydraulic fluid, and distilled water