EPOCAST 1633

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

EPOCAST 1633

Main features

  • Non-Flowing Cartridge Application
  • Flexible Room-Temperature or Heat Cure
  • Honeycomb Fastener Potting

Product Description

EPOCAST 1633 A/B Epoxy Syntactic is a two-component, halogen-free, self-extinguishing medium-paste compound for potting fasteners in honeycomb structures. The system is non-flowing and cartridge-capable, supporting controlled placement in localized potting areas. Part A and Part B mix at 100:50 by weight and may be cured for three days at room temperature or with shorter elevated-temperature schedules after room-temperature gel. Typical cured compressive strength is 6,500 psi, with 1,400 psi tensile lap shear under the stated conditions.

Key features

  • Non-flowing cartridge application: The medium-paste system is cartridge-capable and remains in place after dispensing.
  • Flexible cure schedules: The system supports room-temperature cure or shorter elevated-temperature cycles after gel.
  • Cured mechanical strength: Typical cured compressive strength is 6,500 psi with 1,400 psi tensile lap shear.

Applications

  • Potting fasteners in honeycomb structures
Product Family

EPOCAST 1633

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
White
Pot Life
2-5 minutes
Physical Properties
Viscosity (Part B)
soft-paste mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-received and storage data for the two-component system.

Property Value Unit Method / condition
Appearance Medium paste - As supplied
Flow behavior Non-flowing - As supplied
Mix ratio by weight 100:50 - Part A:Part B
Storage temperature 60 to 90 deg F Original sealed containers
Shelf life 12 months Under the stated storage conditions
Application format Cartridge-capable - Medium-paste system
Technical properties

After-processing / final-state properties

Typical cured properties and cure options for EPOCAST 1633 A/B.

Property Value Unit Method / condition
Cure schedule 3 days at room temperature; or room-temperature gel plus 5 h at 49 deg C; or 2 h at 66 deg C - Typical cure options
Compressive strength 6,500 psi Typical cured material
Tensile lap shear 1,400 psi Typical cured material
Flammability Self-extinguishing - Cured epoxy syntactic