EPOCAP 55137

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

EPOCAP 55137

Main features

  • UL Hazardous-Locations Class I/II Recognition
  • Low-Shrinkage Fuel-Resistant Encapsulation
  • 7,968 psi Tensile Strength

Product Description

EPOCAP® 45137/55137 (formerly EPOCAP® 25137) is a room temperature curing, two-component epoxy potting and encapsulating system specifically designed for low to medium voltage electrical components. It is a filled system that exhibits very low shrinkage and provides robust chemical resistance to various fuels and alcohol/fuel mixtures.

Key features

  • UL recognized for Hazardous Locations: Certified under file TVLE2.E189694 for Class I, Groups A, B, C, and D, as well as Class II, Groups E, F, and G.
  • Chemical and fuel resistance: Delivers reliable durability against exposure to various fuels and alcohol/fuel mixtures.
  • Optimal thermal management: Features a thermal conductivity of 1.2 W/m-K and supports a recommended service temperature of 105°C.

Applications / Suitable for

  • Potting low to medium voltage electrical components.
  • Encapsulation in hazardous locations requiring UL recognition.
  • Applications requiring resistance to fuel and alcohol/fuel mixtures.
Product Family

EPOCAP 55137

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Red
Specific Gravity
1.58 g/cm³
Physical Properties
Viscosity
12,000 (Part 45137) / 40 (Part 55137)* mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Pre-cure processing characteristics of mixed EPOCAP® 45137/55137.

Property Value Unit Method / condition
Appearance / Color (Mixed) Red - -
Mix Ratio (Weight) 100:5.5 - Part 45137 to Part 55137
Mix Ratio (Volume) 100:9 - Part 45137 to Part 55137
Specific Gravity (Mixed) 1.58 - at 25°C
Gel Time 60 minutes 100 gm mass at 25°C
Filler Type Abrasive - Part 45137 uses abrasive filler
Technical properties

After-processing / final-state properties

Typical cured mechanical, thermal, and electrical properties of EPOCAP® 45137/55137 when cured for 7 days at 25°C.

Property Value Unit Method / condition
Hardness 80 Shore D Tested at 25°C
Tensile Strength 7,968 psi Tested at 25°C
Flexural Strength 15,280 psi Tested at 25°C
Heat Distortion Temperature 52.5 °C -
Recommended Service Temperature 105 °C -
Thermal Conductivity 1.2 W/m-K -
Dielectric Strength 358 volts/mil at 1/8" thickness