EPO-TEK 377

Harmonization Code : 3810.10.00 | Soldering, brazing or welding powders and pastes consisting of metal and other materials

EPO-TEK 377

Main features

  • Low-Viscosity Optical Processing
  • 24-Hour Mixed Pot Life
  • High-Transmission Fiber-Optic Epoxy

Product Description

EPO-TEK 377 Epoxy is a two-component, high-Tg fiber-optic-grade epoxy for semiconductor and optical assembly. The pourable system mixes 1:1 by weight, has a typical viscosity of 150 to 300 cP at 23 deg C, and provides a 24-hour pot life. A recommended cure of one hour at 150 deg C develops electrical insulation and optical transmission, including at least 90% transmission from 600 to 1,000 nm. The material is used in fiber-optic, wafer-bonding, capillary-underfill, and other supported optical and semiconductor applications.

Key features

  • Low-viscosity optical processing: Typical viscosity is 150 to 300 cP at 23 deg C and 100 rpm.
  • Extended mixed-material window: The two-component system provides a 24-hour pot life.
  • Optical and electrical performance: Typical cured data include at least 90% transmission from 600 to 1,000 nm and volume resistivity of at least 1 x 10^13 ohm cm.

Applications

  • Fiber-optic assembly
  • Semiconductor and optical packaging
  • Wafer-to-wafer bonding
  • Capillary underfill of flip-chip packages
Product Family

EPO-TEK 377

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Two Part
Refractive index
1.5195
Physical Properties
Viscosity
150 - 300 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
≥ 95 °C
Operating Temperature
< 300 °C
Electrical Properties
Volume Resistivity
≥ 1 x 10¹³ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values apply to the two-component material before cure and to the mixed system where stated.

Property Value Unit Method / condition
Mix ratio by weight 1:1 - Part A:Part B
Specific gravity Part A 1.15; Part B 1.22 - As supplied
Pot life 24 h Mixed system
Shelf life - bulk 1 year At room temperature
Shelf life - syringe 6 months At -40 deg C
Color Part A clear/colorless; Part B amber - Before cure
Consistency Pourable liquid - Before cure
Viscosity 150 to 300 cP At 23 deg C and 100 rpm
Technical properties

After-processing / final-state properties

Typical cured values apply to the stated cure and test conditions.

Property Value Unit Method / condition
Recommended cure 1 h At 150 deg C
Glass transition temperature >= 95 deg C Dynamic cure: 20 to 200 deg C; ISO 25 min; ramp -10 to 200 deg C at 20 deg C/min
Shore D hardness 67 - Typical cured value
Lap shear strength 1,456 psi At 23 deg C
Die shear strength >= 10 kg / 3,556 psi At 23 deg C
Volume resistivity >= 1 x 10^13 ohm cm At 23 deg C
Dielectric constant 3.36 - At 1 kHz
Spectral transmission >= 90 % At 600 to 1,000 nm and 23 deg C
Refractive index 1.5195 - At 589 nm and 23 deg C