Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

EPIBOND 420

Main features

  • Structural Applications Epoxy Bonding
  • Room-Temperature Adhesive Cure
  • Extremely Tough and Resilient

Product Description

Huntsman EPIBOND® 420 A/B Structural Epoxy Adhesive is a two-component, modified epoxy adhesive designed for structural bonding applications requiring high strength, toughness, and resilience. This room-temperature curing paste is suitable for bonding metals, honeycomb structures, and fiber-reinforced composites in demanding assemblies. The adhesive incorporates 5 mil (125 μm) spacer beads to help maintain a consistent bond line in high-stress joints. EPIBOND® 420 A/B offers a practical combination of room-temperature processing flexibility and accelerated heat-cure options, making it suitable for a range of aerospace, industrial, and composite bonding applications.

Key features

  • Structural epoxy formulation: Developed for high-strength bonding of metals, honeycomb materials, and fiber-reinforced composite substrates.
  • Controlled bond-line thickness: Contains 125 μm spacer beads to help maintain a uniform adhesive bond line in high-stress assemblies.
  • Flexible curing options: Supports room-temperature cure or accelerated thermal cure schedules to accommodate different manufacturing requirements.

Applications / Suitable for

  • Metal-to-metal structural bonding
  • Honeycomb panel assembly
  • Fiber-reinforced composite bonding
  • Aerospace structural assemblies
  • Industrial structural adhesive applications
Product Family

EPIBOND 420

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Blue-green
Component System
Two (Resin / Hardener)
Density (g)
1.05 g/cm3

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties for the EPIBOND® 420 A/B adhesive system.

Property Value Unit Method / condition
Mix ratio 100 : 40 wt. ratio 420 A Resin : 420 B Hardener
Density 1.05 g/cm³ ASTM D792, mixed system
Appearance Blue-green — Mixed adhesive system
Work life 70 minutes 77°F (25°C), ASTM D1338
Viscosity Semi-paste — 77°F (25°C), ASTM D2196
Shelf life 1 year Stored at +2°C to +40°C in sealed container
Technical properties

After-processing / final-state properties

Typical cured properties after one hour at 250°F (121°C). Values are typical data and not specifications.

Property Value Unit Method / condition
Lap shear strength 3500 (24.1) psi (MPa) Al-Al, ASTM D1002, 77°F (25°C)
Insert shear strength 1500 (10.3) psi (MPa) As cured, BMS 5-107
Insert shear strength retention 1400 (9.6) psi (MPa) After 30 days at 140°F (60°C), 95% RH, BMS 5-107