Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

EPIBOND 1217

Main features

  • Quick-Set Epoxy Adhesive
  • Room-Temperature Epoxy Cure
  • 1:1 Mix Ratio

Product Description

Epibond® 1217 A/B Epoxy Adhesive is a two-part, translucent epoxy adhesive system designed for rapid bonding of steel, aluminum, wood, ceramics, and a variety of polymeric substrates. This room-temperature-curing adhesive uses a simple 1:1 mix ratio by weight or volume and develops handling strength quickly, making it suitable for fast assembly and repair operations. The material is supplied as a paste and is available in twin-cartridge packaging for dispensing through static mixing equipment. Typical cured lap shear strength on aluminum reaches 2,500 psi (17.2 MPa) at 25°C, providing strong adhesion across a range of common engineering materials.

Key features

  • Fast room-temperature cure: Typical cure is achieved within 1 to 2 hours at 25°C for rapid assembly processes.
  • Simple 1:1 mix ratio: Equal-volume and equal-weight mixing simplifies dispensing and processing.
  • Strong structural bonding: Typical aluminum-to-aluminum lap shear strength reaches 2,500 psi (17.2 MPa) at 25°C.

Applications / Suitable for

  • Bonding steel components
  • Bonding aluminum assemblies
  • Wood bonding applications
  • Ceramic assembly and repair
  • Bonding a variety of polymeric substrates
Product Family

EPIBOND 1217

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Translucent
Density (g)
1.19 g/cm3

Additional Information

Technical properties

As-supplied / before-processing properties

Typical processing and material properties for the supplied resin, hardener, and mixed adhesive system.

Property Value Unit Method / condition
Mix ratio 1:1 Volume / Weight Part A : Part B
Density (mixed) 1.19 g/cm³ ASTM D792, 25°C
Gel time 4-8 minutes 50 g sample at 25°C
Appearance Translucent - Mixed system, visual
Typical cure cycle 1-2 hours 25°C
Technical properties

After-processing / final-state properties

Typical cured adhesive performance values measured on aluminum test specimens.

Property Value Unit Method / condition
Tensile lap shear 2,500 (17.2) psi (MPa) ASTM D1002, Al-Al, 25°C
Tensile lap shear 1,350 (9.3) psi (MPa) ASTM D1002, Al-Al, -55°C
Tensile lap shear 500 (3.4) psi (MPa) ASTM D1002, Al-Al, 83°C