ENTHONE B3

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

ENTHONE B3

Main features

  • Four-Hour Ink Pot Life
  • Controlled Heat-Cure Processing
  • Faster Cure at Higher Temperature

Product Description

ENTHONE B-3 Catalyst is a heat-cure-only catalyst component for ENTHONE M-Series epoxy marking inks. It provides an average 4-hour pot life after the specified induction period, giving a defined processing window before the ink begins to solidify. Cure temperature must exceed 79 deg C, and higher temperatures shorten the required cure time within the published ink-film schedule. B-3 is used where permanent epoxy markings are processed through controlled thermal cure, including supported M-Series color packages and premeasured bi-pack configurations.

Key features

  • Heat-Cure-Only Processing: B-3 is used exclusively with controlled thermal cure.
  • Four-Hour Pot Life: The catalyzed ink has an average 4-hour working pot life after induction.
  • Temperature-Responsive Cure: Higher cure temperatures reduce the required ink-film cure time.

Applications / Suitable for

  • ENTHONE M-Series heat-cured marking inks
  • M 0 N and M 9 N bi-pack configurations
  • M 0 NC nonconductive black bi-pack configurations
Product Family

ENTHONE B3

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Amber Liquid
Thermal Properties
Boiling Point
160 °C
Flash Point
73.889 °C
Physical Properties
VOC
720 g/l

Additional Information

Technical properties

As-supplied / before-processing properties

Typical catalyst and catalyzed-ink processing data. Final properties belong to the selected M-Series ink, catalyst ratio, and cure schedule.

Property Value Unit Method / condition
Catalyst function Basic heat-cure catalyst - ENTHONE M-Series epoxy marking inks
Cure mode Heat only - B-3 catalyst
Average pot life 4 hr Begins after induction period
Induction period 30 min All standard catalysts, including B-3
Required cure temperature >79 deg C Above 175 deg F
Shelf life 2 years All ENTHONE catalysts; from date of manufacture