ENTHONE AD2002

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

ENTHONE AD2002

Main features

  • Spray-Application Viscosity Control
  • Air-Pressure and Orifice Adjustment
  • Extended Catalyzed-Ink Pot Life

Product Description

ENTHONE AD2002 Thinner is a process additive used to prepare ENTHONE M-Series and 50-Series epoxy marking inks for spray application. It is added after the catalyst induction period, with the amount adjusted to spray-unit air pressure and orifice. The M-Series guide specifies 25 to 40% by volume; the 50-Series guide allows 25 to 50% by volume. AD2002 extends the catalyzed ink pot life considerably and may also be used for localized equipment cleaning before the ink dries or partially cures.

Key features

  • Spray-Application Thinning: AD2002 adjusts catalyzed ENTHONE inks for spray equipment and atomization conditions.
  • Ink-Specific Addition Ranges: Addition is 25 to 40% by volume for M-Series and 25 to 50% for 50-Series.
  • Extended Pot Life: Thinner addition substantially lengthens the catalyzed ink working period.

Applications / Suitable for

  • ENTHONE M-Series spray application
  • ENTHONE 50-Series spray application
  • Localized marking-equipment cleaning before partial cure
Product Family

ENTHONE AD2002

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear Liquid
Vapor Density
>1 (Air =1)
Vapor Pressure
16 mmHg
Thermal Properties
Boiling Point
115.5 °C
Flash Point
21.111 °C
Physical Properties
VOC
910 g/l

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied and spray-processing data for AD2002. Addition ranges depend on the selected ENTHONE ink family and spray equipment.

Property Value Unit Method / condition
Physical state Liquid - As supplied
M-Series addition 25 to 40 vol% After induction; adjust for spray air pressure and orifice
50-Series addition 25 to 50 vol% After induction; adjust for spray air pressure and orifice
Relative density 0.901 - As-supplied measurement
Storage temperature 5 to 40 deg C As-supplied condition