ENTHONE 20/A

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

ENTHONE 20/A

Main features

  • Two-Hour Mixed-Ink Pot Life
  • Ambient or Heat Cure
  • Permanent Marking Application Flexibility

Product Description

ENTHONE Catalyst 20/A is an ambient- or heat-cure catalyst component for ENTHONE M-Series and 50-Series two-component epoxy marking inks. With the selected ink, the mixture has an average 2-hour pot life after a 30-minute induction period. A room-temperature air cure reaches tack-free condition in approximately 1 to 2 hours and develops over 5 to 7 days, while heat cure is also available. The catalyst supports permanent marking processes for semiconductor components, printed circuit boards, connectors, dials, nameplates, panels, chassis, glass, and compatible plastics.

Key features

  • Two-Hour Mixed Pot Life: The ink and Catalyst 20/A mixture has an average 2-hour pot life after induction.
  • Ambient or Heat Cure: The selected ink system may cure at room temperature or through a heat-assisted schedule.
  • Multi-Method Marking: Compatible inks may be stamped, screen printed, sprayed, brushed, or roller printed.

Applications / Suitable for

  • Permanent marking of semiconductor components
  • Printed circuit boards, connectors, and dials
  • Nameplates, panels, chassis, glass, and compatible plastics
Product Family

ENTHONE 20/A

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Basic air cure catalyst

Additional Information

Technical properties

As-supplied / before-processing properties

Typical processing data for Catalyst 20/A used with M-Series or 50-Series epoxy marking inks.

Property Value Unit Method / condition
Induction period 30 minutes Ink/catalyst mixture before application
Average pot life 2 hours Catalyst 20/A with M-Series or 50-Series ink; begins after induction
Tack-free time 1 to 2 hours Room-temperature air cure; depends on ink film thickness
Room-temperature cure 5 to 7 days Catalyst 20/A with ENTHONE epoxy marking ink
Cure mode Room temperature or heat - Catalyst 20/A may be fully or partially heat cured
Catalyst shelf life 2 years From date of manufacture
Moisture handling Keep tightly closed - Catalysts are hygroscopic