ELANTAS UC-54

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

ELANTAS UC-54

Main features

  • Direct 100% Solids Mold Filling
  • Tough High-Impact Prototypes
  • Thermoplastic-Style Surface and Feel

Product Description

CONATHANE UC-54 Two-Component Casting Urethane is an unfilled, 100% solids two-component urethane for castings and prototype parts. The reactive liquid system forms tough, high-impact, dimensionally stable components with a thermoplastic-like feel and appearance. Its 100% solids formulation supports direct mold filling after the two components are combined, while the casting route provides a practical way to produce prototype and molded urethane shapes. UC-54 is suited to cast parts where impact response, dimensional stability, and a thermoplastic-style surface are important selection factors.

Key features

  • 100% Solids Casting: The unfilled material is supplied as a 100% solids two-component casting system.
  • Tough Prototype Parts: UC-54 is positioned for tough, high-impact castings and prototypes.
  • Thermoplastic-Like Finish: The cured material provides a thermoplastic-style feel and appearance.

Applications / Suitable for

  • Prototype urethane parts
  • Tough, high-impact castings
  • Castings requiring thermoplastic-like feel and appearance
Product Family

ELANTAS UC-54

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Flash Point
94 °C
Glass Transition Temperature (Tg)
98 °C
General Properties
Appearance
translucent white
Mechanical Properties
Elongation
8 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of CONATHANE® UC-54 components and mixed material prior to cure.

Property Value Unit Method / condition
Viscosity 500 / 2,000 cP Part A / Part B at 25°C
Specific Gravity 1.18 / 1.08 - Part A / Part B at 25°C
Mix Ratio 100 : 50 Parts by weight Part A : Part B
Mixed Viscosity (Initial) 1,200 cP Mixed material at 25°C
Work Life 45 minutes 200 g mass at 25°C
Technical properties

After-processing / final-state properties

Typical cured-material physical properties following the recommended cure schedule.

Property Value Unit Method / condition
Shore Hardness D85 Shore D ASTM D2240, 25°C
Tensile Strength 12,260 psi ASTM D412, 25°C
Ultimate Elongation 8 % ASTM D638, 25°C
Glass Transition Temperature 98 °C Typical value
Linear Shrinkage 0.45 % ASTM D2566, 16 h at 80°C