ELANTAS TU-6090

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ELANTAS TU-6090

Main features

  • Equal-Volume Two-Part Mixing
  • Fifteen-to-Twenty-Minute Work Life
  • Shore A 90 Tooling Elastomer

Product Description

CONATHANE TU-6090 Two-Component Polyurethane Casting System is an unfilled, 100% solids two-component polyurethane tooling elastomer for casting flexible parts. Part A and Part B are mixed at 100/50 by weight or volume, producing a typical mixed viscosity of 3,100 cP at 25 deg C and a 15 to 20 minute work life. The system cures for 7 to 10 days at 25 deg C or 16 hours at 60 deg C. The cured elastomer reaches Shore A 90 hardness, 2,850 psi tensile strength, and 335% elongation.

Key features

  • Equal Weight-or-Volume Ratio: The 100/50 mix ratio applies by weight and by volume.
  • Fifteen-to-Twenty-Minute Work Life: The mixed system has a typical 15 to 20 minute processing window at 25 deg C.
  • Shore A 90 Elastomer: The cured tooling elastomer combines Shore A 90 hardness with 335% elongation.

Applications / Suitable for

  • Industrial wheels and rolls
  • Metal-forming pads and flexible molds
  • Washers, gaskets, bushings, and vibration-dampening pads
Product Family

ELANTAS TU-6090

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
light amber
Mechanical Properties
Elongation
335 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component, mixing, degassing, work-life, and cure data for TU-6090.

Property Value Unit Method / condition
Component viscosity Part A: 4,000; Part B: 1,350 cP Typical at 25 deg C
Component specific gravity Part A: 1.04; Part B: 1.05 - Typical at 25 deg C
Mix ratio 100/50 parts Part A / Part B; by weight or by volume
Initial mixed viscosity 3,100 cP Typical at 25 deg C
Work life 15 to 20 minutes Typical at 25 deg C
Component preheat Up to 60 deg C Optional processing aid before mixing
Vacuum degassing >27 in Hg Recommended after mixing when degassing is used
Cure schedule 7 to 10 days or 16 hours - At 25 deg C or 60 deg C
Technical properties

After-processing / final-state properties

Typical cured mechanical properties for the TU-6090 tooling elastomer.

Property Value Unit Method / condition
Hardness 90 Shore A Typical cured property
Tensile strength 2,850 psi Typical cured property
100% modulus 1,000 psi Typical cured property
300% modulus 2,800 psi Typical cured property
Elongation 335 % Typical cured property
Tear strength 390 pli Typical cured property