ELANTAS EN-16

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ELANTAS EN-16

Main features

  • Cartridge-Friendly Four-to-One Mixing
  • Defined 30-Minute Working Window
  • High-Elongation Cured Potting

Product Description

CONATHANE EN-16 Two-Component Polyurethane Potting Compound is an unfilled, 100% solids polyether-based polyurethane system for harness breakouts, watertight connectors, cables, and cable-end seals. The 4:1 mix ratio by weight and volume produces a 4,000 cP mixed material with a 30-minute work life at 25 deg C. Cure may be completed in 7 days at 25 deg C or 16 hours at 80 deg C. The cured elastomer reaches Shore A 80, 510% ultimate elongation, and 4,200 psi tensile strength, supporting flexible, abrasion-resistant potting and molded electrical applications.

Key features

  • Cartridge-Friendly 4:1 Mixing: The four-to-one volumetric ratio supports controlled cartridge or meter-mix processing.
  • 30-Minute Work Life: The mixed compound provides a defined processing window at 25 deg C.
  • High Cured Elongation: Typical 510% ultimate elongation provides a flexible final elastomer profile.

Applications / Suitable for

  • Harness breakouts
  • Watertight electrical connectors
  • Cables and cable-end seals
  • Abrasion-resistant mechanical castings
Product Family

ELANTAS EN-16

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Amber
Mechanical Properties
Elongation
510 %
Chemical Properties
Moisture absorption
2.6 %
Electrical Properties
Dielectric Strength
18.90 kV/mm
Surface Resistivity
1.7 x 10^14 Ohms/sq
Volume Resistivity
1.4 x 10^12 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied and processing characteristics used for material and process evaluation. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Part A / Part B viscosity 5,880 / 520 cP At 25 deg C
Part A / Part B specific gravity 1.06 / 1.06 - At 25 deg C
Mix ratio by weight 100:25 parts Part A to Part B
Mix ratio by volume 100:25 parts Part A to Part B
Initial mixed viscosity 4,000 cP At 25 deg C
Work life 30 minutes At 25 deg C
Cure schedules 7 days at 25 deg C or 16 hours at 80 deg C - Time after the unit reaches the specified temperature
Technical properties

After-processing / final-state properties

Final-state characteristics after the stated cure or processing condition. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Shore hardness A 80 - ASTM D2240 at 25 deg C
Compression set 44 % ASTM D395 Method B
Tensile strength 4,200 psi ASTM D412 at 25 deg C
Ultimate elongation 510 % ASTM D412 at 25 deg C
Tear strength 420 pli ASTM D624 at 25 deg C
Dielectric strength 480 V/mil ASTM D149; 1/16 in specimen at 25 deg C
Volume resistivity 1.4 x 10^12 ohm cm ASTM D257 at 25 deg C