ELANTAS EN-14

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ELANTAS EN-14

Main features

  • Equal-Volume Meter-Mix Processing
  • Defined 20-Minute Working Window
  • Flexible Thermal-Shock-Resistant Encapsulation

Product Description

CONATHANE EN-14 Two-Component Polyurethane Potting Compound is an unfilled, 100% solids polyurethane system for potting and encapsulating electrical and electronic assemblies. A 1:1 volumetric mix produces an initial mixed viscosity of 1,200 cP and a 20-minute work life at 25 deg C for controlled casting or meter-mix processing. Cure can proceed for 3 to 4 days at 25 deg C or 3 hours at 60 deg C. The cured material combines Shore A 65 hardness, 110% elongation, 0.2 W/(m K) thermal conductivity, and passes 10 thermal-shock cycles from -65 to 130 deg C.

Key features

  • Controlled 1:1 Mixing: Equal-volume mixing supports bench, meter-mix, or vacuum potting processes.
  • 20-Minute Working Window: The mixed material provides a defined work life at 25 deg C before gelation.
  • Flexible Cured Encapsulation: Shore A 65 hardness and 110% elongation provide a flexible final material profile.

Applications / Suitable for

  • Potting electrical assemblies
  • Encapsulating electronic assemblies
Product Family

ELANTAS EN-14

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Thermal Conductivity
0.2 W/m.K
UL 94 Rating
V2
Mechanical Properties
Elongation
110 %
Electrical Properties
Arc Resistance
>120 s
Dielectric Strength
19.7 kV/mm
Surface Resistivity
1 x 10^13 Ohms/sq
Volume Resistivity
3 x 10^13 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied and processing characteristics used for material and process evaluation. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Part A / Part B viscosity 1,500 / 1,000 cP At 25 deg C
Mix ratio by weight 100:90 parts Part A to Part B
Mix ratio by volume 100:100 parts Part A to Part B
Initial mixed viscosity 1,200 cP At 25 deg C
Gel time 15 minutes At 25 deg C
Work life 20 minutes At 25 deg C
Cure schedules 3 to 4 days at 25 deg C or 3 hours at 60 deg C - Time after the unit reaches the specified temperature
Technical properties

After-processing / final-state properties

Final-state characteristics after the stated cure or processing condition. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Shore hardness A 65 - ASTM D2240 at 25 deg C
Tensile strength 700 psi ASTM D229 at 25 deg C
Elongation 110 % ASTM D229 at 25 deg C
Thermal conductivity 0.2 W/(m K) ASTM C177
Thermal shock Pass, 10 cycles - -65 to 130 deg C
Dielectric strength >500 V/mil ASTM D149 at 25 deg C
Volume resistivity 3 x 10^13 ohm cm ASTM D257 at 25 deg C