ELANTAS CE-1155-35

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

ELANTAS CE-1155-35

Main features

  • Extended Eight-to-Ten-Hour Pot Life
  • UV-Fluorescent Coverage Inspection
  • Flexible Electrical Moisture Barrier

Product Description

CONATHANE CE-1155-35 Two-Component Polyurethane Conformal Coating is a transparent, pre-diluted polyurethane system for forming thin electrical and moisture barriers on components and printed circuit boards. The 1:1 volumetric mix produces a 25 cP coating with an 8 to 10 hour pot life for spray, dip, or brush application. A minimum two-coat process targets a total cured film thickness of 2 mil with a tolerance of 1 mil. The cured coating remains flexible, fluoresces under UV light for inspection, and passes hydrolytic-stability and thermal-shock tests under MIL-I-46058C conditions.

Key features

  • Extended Coating Pot Life: An 8 to 10 hour pot life at 25 deg C supports sustained spray, dip, or brush processing.
  • UV-Fluorescent Inspection: Tracer dye makes the applied coating fluorescent under UV light for coverage checks.
  • Flexible Environmental Barrier: The cured film passes hydrolytic-stability and thermal-shock tests.

Applications / Suitable for

  • Thin-film electrical and moisture barrier for components
  • Printed circuit board conformal coating
Product Family

ELANTAS CE-1155-35

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
clear amber
Other Properties
RoHS Compliant
Yes

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied and processing characteristics used for material and process evaluation. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Mix ratio 100:100 parts by volume Part A to Part B
Part A viscosity 30 cP At 25 deg C
Part B viscosity 20 cP At 25 deg C
Part A / Part B specific gravity 1.05 / 0.93 - At 25 deg C
Mixed viscosity 25 cP Brookfield at 25 deg C
Pot life 8 to 10 hours At 25 deg C
Technical properties

After-processing / final-state properties

Final-state characteristics after the stated cure or processing condition. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Total cured film thickness 2 with a tolerance of 1 mil Minimum two-coat process
Hydrolytic stability No discoloration or degradation - MIL-I-46058C; 120 days at 85 deg C and 95% RH
Flexibility Pass - MIL-I-46058C; 1/8 in diameter mandrel
Thermal shock Pass - MIL-I-46058C; -65 to 125 deg C
Insulation resistance >2.5 x 10^13 ohm MIL-I-46058C; 2 mil at 25 deg C and 50% RH
Volume resistivity 1.2 x 10^16 ohm cm ASTM D257 at 25 deg C