ELANTAS AD-1161

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ELANTAS AD-1161

Main features

  • PVC-to-Polyurethane Adhesion Priming
  • Fast 30-Minute Air-Dry Step
  • MIL-M-24041 QPL-Listed Primer

Product Description

CONAP AD-1161 Adhesive Primer is a light-amber, solvent-borne modified phenolic primer for bonding liquid polyurethane systems to prepared polyvinyl chloride surfaces. The 80 cP liquid can be applied by brush, spray, or roller, then air dried for 30 minutes at room temperature before polyurethane placement. Typical peel strength reaches 30 pli with EN-1554 and EN-1556 polyurethane systems on prepared PVC. The primer is QPL listed to MIL-M-24041 Category B, Type I and is supplied with a 12-month storage period at or below 25 deg C.

Key features

  • PVC-Specific Adhesion Priming: The primer supports liquid polyurethane bonding to properly prepared polyvinyl chloride.
  • 30-Minute Air Dry: A defined room-temperature air-dry step supports controlled polyurethane application.
  • Qualified Primer Scope: QPL listing to MIL-M-24041 Category B, Type I preserves the exact qualification scope.

Applications / Suitable for

  • Liquid polyurethane bonding to prepared PVC surfaces
Product Family

ELANTAS AD-1161

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
light amber
Solids
20 %
Physical Properties
Viscosity
80 mPa.s
Thermal Properties
Flash Point
-9 °C
Other Properties
RoHS Compliant
Yes

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied and processing characteristics used for material and process evaluation. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Appearance Light amber - As supplied
Viscosity 80 cP At 25 deg C
Solids content 20 % Typical as supplied
Adjustment solvent MEK - For application adjustment where required
Weight per gallon 7.3 lb/gal Typical as supplied
Flash point -9 deg C ASTM D93
Shelf life 12 months Stored at or below 25 deg C