LOCTITE ECCOBOND UV8800M-X
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other
Main features
- Fast UV Cure
- Good workability
- Good adhesion
Product Description
LOCTITE ECCOBOND UV8800M-X encapsulant is formulated for use in smart card applications. It cures to form a hard translucent coating when exposed to UV light of sufficient intensity. The curing of the product is not inhibited by oxygen, resulting in excellent surface cure.
LOCTITE ECCOBOND UV8800M-X glob top encapsulant can be used on FR4, FCI and LG tape substrates.
UV Cure
- Light Intensity, mW/cm2 100
- Exposure Time, seconds 30
TDS, SDS & Technical Documents
Technical Specifications
Thermal Properties
Glass Transition Temperature (Tg)
47 °C
Physical Properties
Thixotropic index
1.1
Viscosity
3,400 mPa.s