LOCTITE ECCOBOND UF4550HTC

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND UF4550HTC

Main features

  • Thermally conductive
  • Low ionics
  • Alumina filled

Product Description

LOCTITE ECCOBOND UF 4550HTC is a board level capillary underfill designed to provide enhanced thermal properties and adhesion to integrated circuit passivation material and flex circuits. LOCTITE ECCOBOND UF 4550HTC is designed to quickly underfill at elevated substrate temperature of 90 to 110°C.

LOCTITE ECCOBOND UF 4550HTC provides thermal conductivity for applications where thermal management is required. This material is also engineered to provide good thermal cycle reliability for PCBAs.

Cure Schedule

  • 15 minutes @ 160°C
Product Family

ECCOBOND UF4550HTC

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 23 days
CA Shipping in 12 weeks
EU Shipping in 45 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
2.47
Thermal Properties
Glass Transition Temperature (Tg)
143 °C
Thermal Conductivity
1 W/m.K
Chemical Properties
Moisture absorption
0.5 %
Physical Properties
Thixotropic index
0.9
Viscosity
12,000 mPa.s