LOCTITE ECCOBOND MC723

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND MC723

Main features

  • Ultra low moisture absorption
  • For Flip chip BGA
  • Soon to be discontinued

Product Description

We regret to inform you that MC723 won't be supplied from September 1st 2025 onwards. A raw material discontinuation and the limited volumes cannot justify spending resources to continue supplying this.

Some close alternatives that you might want to consider are ABP 2035SCR, next to 2025D (lower modulus, successful in lid attach) and or QMI 536HT (~1 W/m-K) depending on your application description and test requirements.


LOCTITE ECCOBOND MC 723
 silicone adhesive is designed for lid attach in flip chip BGA applications. The ultra low moisture absorption at environmental and reliability conditions ensure high reliability performance in advanced laminate packages.

LOCTITE ECCOBOND MC 723 is a non conductiveadhesive with very fast curing kinetics in conventional box oven. This adhesive can be applied on organic, metals and laminates and is typically used for ball grid arrays applications.

Recommended Cure

  • 30 minute ramp to 150°C + 30 minutes @ 150°C
  • 30 minute ramp to 165°C + 30 minutes @ 165°C
Product Family

ECCOBOND MC723

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
10 hours
Thermal Properties
Glass Transition Temperature (Tg)
42 °C
Thermal Conductivity
0.8 W/m.K
Physical Properties
Thixotropic index
1.5
Viscosity
57,000 mPa.s

Leading Brands Trust in Our Products and Services