LOCTITE ECCOBOND LUX A4035T

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND LUX A4035T

Main features

  • Photocurable
  • Pale yellow
  • Photodiode and Optical fiber terminations

Product Description

LOCTITE ECCOBOND LUX A4035T photocurable acrylate adhesive is formulated to enhance productivity in the assembly of optical, fiber optic, and optoelectronic devices. In addition to light cure, this adhesive contains a secondary thermal cure initiator.

LOCTITE ECCOBOND LUX A4035T is an optical grade, pale yellow acrylate that can achieve  a thin bondline. It is typically used for photodiode arrays and optical fiber terminations.

 

UV Cure

  • UV or visible light

Secondary Thermal Cure

  • 1 hour @ 100°C or
  • 2 hours @ 80°C
Product Family

ECCOBOND LUX A4035T

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 18 days
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Refractive index
1.55
Thermal Properties
Glass Transition Temperature (Tg)
145 °C
Physical Properties
Viscosity
500 mPa.s