LOCTITE ECCOBOND FP4547

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND FP4547

Main features

  • Enhanced adhesion
  • Rigid, low stress seal
  • High purity

Product Description

LOCTITE ECCOBOND FP4547 liquid epoxy underfill is designed to provide enhanced adhesion to integrated circuit passivation materials. This material is formulated to quickly underfill devices at 90 to 120°C substrate temperature, with as little as a 2 to 3 mil gap.

When fully cured, the material forms a rigid, low stress seal that dissipates stress on solder joints and extends thermal cycling performance. LOCTITE ECCOBOND FP4547 also exhibits low moisture absorption for improved JEDEC performance.

Recommended Cure Schedule

  • 30 minutes @ 165°C
Product Family

ECCOBOND FP4547

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 50 days
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Glass Transition Temperature (Tg)
135 °C
Physical Properties
Viscosity
18,000 mPa.s