Product Description
LOCTITE ECCOBOND FP4451 is the industry standard damming material, designed as a flow control barrier around areas of bare chip encapsulation.
LOCTITE ECCOBOND FP4451 is designed to be used in combination with FP4450 fill encapsulant. It passes pressure pot performance on live devices up to 500 hours with no failures depending on device and package type.
Recommended Cure Schedule
- 30 minutes @ 125°C plus
- 90 minutes @ 165°C
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Pot Life
48 hours
Specific Gravity
1.76
Thermal Properties
Glass Transition Temperature (Tg)
155 °C
Other Properties
MSL Level
MSL 2
Physical Properties
Viscosity
1,300,000 mPa.s