ECCOBOND F123

Harmonization Code : 5906100000 | Adhesive tape of a width not exceeding 20cm

ECCOBOND F123

Main features

  • Fast Application Cure
  • Good Capillary Application
  • Thermal Shock Resistance

Product Description

LOCTITE ECCOBOND F 123 is a two-part, heat-cure epoxy adhesive formulated for terminating single- and multi-channel fiber optic connectors and potting glass fibers and fiber optic bundles. The mixed material has a typical viscosity of 4,000 cP at 25°C and a four-hour pot life, supporting controlled wicking into optical assemblies. It uses a 100:10 resin-to-hardener mix ratio by weight and offers cure schedules as fast as one minute at 150°C. The cured adhesive operates from -60 to 175°C and combines mechanical-impact resistance, thermal-shock resistance, and low-stress bonding with no pistoning. Its color-keyed formulation changes from green/blue when mixed to reddish-amber after cure, providing a visible indication of cure status.

Key features

  • Fast heat cure: Cure options include five minutes at 100°C, two minutes at 120°C, or one minute at 150°C.
  • Low-viscosity wicking: Typical mixed viscosity of 4,000 cP at 25°C supports application within fiber optic assemblies.
  • Low-stress optical bonds: Resists mechanical impact and thermal shock while supporting connections without pistoning.

Applications / Suitable for

  • Single- and multi-channel fiber optic connector termination
  • Fiber optic bundle assembly
  • Potting glass fibers
Product Family

ECCOBOND F123

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Thixotropic index
1.0
Viscosity
4000 mPa.s
General Properties
Mix Ratio
100:10
Refractive index
1.56
Specific Gravity
1.2
Thermal Properties
Glass Transition Temperature (Tg)
120 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values unless stated otherwise. Mixed properties apply after combining resin and hardener at a 100:10 ratio by weight.

Property Value Unit Method / condition
Appearance Light yellow — Unmixed material
Appearance Green/blue — Completely mixed material
Mix ratio 100:10 Ratio Resin to hardener, by weight
Mixed viscosity 4,000 cP At 25°C
Specific gravity 1.2 — Mixed material
Pot life 4 hours Mixed material
Reactive solids content 100 % Typical uncured material property
Technical properties

After-processing / final-state properties

Typical cured-material and bonded-joint reference values. Results are not guaranteed production specifications or universal joint-design values.

Property Value Unit Method / condition
Operating temperature -60 to 175 °C Documented product operating range
Glass transition temperature 120 °C Typical cured material
Hardness 87 Shore D Typical cured material
Refractive index 1.56 — Typical cured material
Water absorption 0.004 % Typical cured material
Spectral transmittance 93 % Wavelength range of 6,000–9,000 Å
Dielectric strength 400 V/mil Typical cured material
Lap shear strength 2,900 psi Aluminum-to-aluminum test specimen