ECCOBOND F113

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ECCOBOND F113

Main features

  • Low-Viscosity Precision Application
  • Optically Clear Material
  • High Surface Wettability

Product Description

LOCTITE ECCOBOND F 113 is a two-part, optically clear epoxy adhesive for bonding and small-volume potting of optical assemblies. The 100:30 resin-to-hardener system has a mixed viscosity of 180 cP at 25 °C, providing low-viscosity flow and excellent wettability around plastic or glass optical fibers, lenses, prisms and LED displays. The cured adhesive has a refractive index of 1.55 and 97% spectral transmittance from 3,200 to 9,000 Å. It can be cured for 24 hours at 25 °C or accelerated for 1 to 2 hours at 65 °C, with a documented operating temperature range of -60 to 100 °C. It bonds glass, glass fibers, ceramics, many metals and most rigid plastics.

Key features

  • Optically clear: Provides 97% spectral transmittance from 3,200 to 9,000 Å and a refractive index of 1.55.
  • Low mixed viscosity: A typical viscosity of 180 cP at 25 °C supports wetting and small-volume optical-component potting.
  • Wide operating range: Suitable for operating temperatures from -60 to 100 °C.

Applications / Suitable for

  • Plastic and glass optical fiber bonding
  • Lens and prism bonding
  • LED display assembly
  • Small-volume potting of optical components
Product Family

ECCOBOND F113

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Thixotropic index
1.0
Viscosity
180 mPa.s
General Properties
Mix Ratio
100:30
Refractive index
1.55
Specific Gravity
1.22
Thermal Properties
Glass Transition Temperature (Tg)
45 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured, mixed-material and cure values provided for product evaluation. These values are not guaranteed specifications.

Property Value Unit Method / condition
Appearance Clear — Epoxy adhesive system
Mix ratio 100:30 Parts by weight Resin:hardener
Mixed viscosity 180 cP At 25 °C
Thixotropic index 1.0 — Uncured material
Specific gravity 1.22 — Uncured material
Pot life 2 h Mixed adhesive
Work life 3 h Mixed adhesive
Cure schedule 24 / 1–2 h At 25 °C / 65 °C; guideline cure profiles
Technical properties

After-processing / final-state properties

Typical cured-material properties and laboratory performance values. Test conditions are retained where supplied; values are not guaranteed specifications.

Property Value Unit Method / condition
Operating temperature -60 to 100 °C Documented operating range
Coefficient of thermal expansion 55 ppm/°C Cured material
Glass-transition temperature 45 °C DMA
Refractive index 1.55 — Cured material
Spectral transmittance 97 % From 3,200 to 9,000 Å
Dielectric strength 430 V/mil Cured material
Volume resistivity 9 × 108 Ω·cm At 25 °C
Lap-shear strength 4,000 psi Aluminum/aluminum; cured for 2 h at 65 °C