LOCTITE ECCOBOND EO7021

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Loctite Eccobond EO7021

Main features

  • Fast cure
  • Glob top
  • Die attach & Encapsulant

Product Description

LOCTITE® ECCOBOND EO7021 one component encapsulant is designed for use in smart card chip module applications. It cures fast at moderate temperatures and is also suitable for die attach automated reel to reel processing. It's a good and very reasonably priced die attach/encapsulation combination similar to EO7029.

LOCTITE® ECCOBOND EO7021 has great compatibility with the newly formulated LOCTITE ABLESTIK ABP 2035SCR which and has been improved to be compatible with UV-curable smart card encapsulants.

Product Family

ECCOBOND EO7021

1. Select Package Type
2. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 35 days
Packaging
Please select Package Type and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
1.19
Thermal Properties
Glass Transition Temperature (Tg)
125 °C
Mechanical Properties
Elongation
3.97 %
Physical Properties
Viscosity
17,000 mPa.s

Additional Information

Recommended Cure for Reel-to-Reel Processing

  • Substrate and Chip Module Preheat, ºC 100
  • Precure 3 minutes @ 140°C
  • Postcure (after reel is completely full) 16 hours @ 100°C

Alternate Cure for Reel-to-Reel Processing

  • Precure 1 hour @ 100°C
  • Postcure 6 hours @ 120°C

This applies only to coating chip module with 10 to 100 mg of LOCTITE EO7021.

Recommended Cure for Non-Conductive Die Attach Application

  • 1 hour @ 120°C or
  • 5 minutes @ 150°C