LOCTITE ECCOBOND EO1062
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other
Main features
- Low flow
- Non conductive
- Excellent reliability
Product Description
LOCTITE ECCOBOND EO 1062 is designed to pass 1,000 hours of temperature/humidity/bias testing and thermal cycling up to 125°C. Exceptional viscosity stability at 25°C provides easier control of shot size using conventional time/pressure dispensing equipment.
Cure Schedule
- 4 to 6 hours @ 125°C - Robust non-stress sensitive components
- 3 hours @ 140°C. - Stress sensitive components
Packaging
Please select Package Type and Package Size.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Pot Life
600 hours
Specific Gravity
1.78
Thermal Properties
Glass Transition Temperature (Tg)
125 °C
Electrical Properties
Volume Resistivity
1.90000000000000 Ohms⋅cm
Physical Properties
Viscosity
64,000 mPa.s