LOCTITE ECCOBOND EO1016

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Loctite Eccobond EO1016 LOCTITE ECCOBOND EO1016 LOCTITE ECCOBOND EO1016

Main features

  • Glob top Encapsulant
  • Smartcard applications
  • Fast curing

Product Description

LOCTITE® ECCOBOND EO1016 is an epoxy encapsulant intended for applications requiring excellent handling properties. The cured material survives severe thermal shock and offers continuous service to 177 °C. It is particularly suited for use on transistors and similar semiconductors, can be used for encapsulation of watch ICs. Additionally it exhibits a UL94V-0 rating and its non abrasive filler allows for grinding when this is necessary. It is an ideal product for glob top smartcard encapsulation.

LOCTITE® ECCOBOND EO1016 was used for years in the Swiss Watch making industry and was the Glob Top used to encapsulate the Watch ICs. An important difference with this product is that it is a "EO" family which stands for "Epoxy One Component" which means that it is premixed and refrigerated. The storage temperature of this product is only refrigerated 5C as opposed to the more reactive -40C products.

Cure Schedule

  • 20 minutes @ 150°C
  • 24 hours @ 93°C
Product Family

ECCOBOND EO1016

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot Life
2184 hours
Specific Gravity
1.56
Thermal Properties
Glass Transition Temperature (Tg)
126 °C
Thermal Conductivity
0.39 W/m.K
Mechanical Properties
Elongation
1.8 %
Physical Properties
Thixotropic index
1.1
Viscosity
62,000 mPa.s

Additional Information

We have internal information showing that these legacy materials pass UL94V0 but do not have the test data or yellow card nor are we going to test for it. This is anecdotal but, hopefully, helpful.