LOCTITE ECCOBOND 50400-1

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Loctite Eccobond 50400-1

Main features

  • Low viscosity
  • Low CTE
  • One component

Product Description

LOCTITE® ECCOBOND 50400-1 glob top is designed for encapsulating wire bonded bare die on epoxy laminate and similar substates. The formulation of this single component material ensures a long pot and a very stable, low viscosity during use.

LOCTITE® ECCOBOND 50400-1 is recommended for use on ICs with high wire profiles and in applications where the spreading of the glob top during cure must be controlled.

 

Cure Schedule

  • 2 hours @ 150°C

Low Stress Cure Schedule

  • 1 hour @ 120°C + 1 hour @ 150°C
Product Family

ECCOBOND 50400-1

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 20 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot Life
168 hours
Thermal Properties
Glass Transition Temperature (Tg)
140 °C
Thermal Conductivity
0.63 W/m.K
Physical Properties
Viscosity
100 mPa.s