DYMAX 984-LVF

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DYMAX 984-LVF

Main features

  • One-Part 100% Solids Application
  • UV and Shadow-Area Heat Cure
  • Fluorescent Coating Coverage Inspection

Product Description

Dymax Multi-Cure 984-LVF Conformal Coating is a single-component, 100% solids conformal coating for electronic assemblies. UV light cures exposed areas, while secondary heat cure addresses material in shadowed regions. The fluorescent response helps operators confirm coverage after application, and the one-part format avoids mixing before dispense. The coating is suited to metal, ceramic, and glass-filled epoxy surfaces within electronic assemblies, forming a protective layer without solvent evaporation. Its combined cure routes support complex geometry where not every coated area receives direct light.

Key features

  • One-Part 100% Solids Application: The coating requires no component mixing and cures without solvent evaporation.
  • Dual Cure for Complex Geometry: UV cure is complemented by secondary heat cure in shadowed areas.
  • Fluorescent Coverage Check: Fluorescence supports visual confirmation of the applied coating.

Applications / Suitable for

  • Conformal coating on metal surfaces
  • Conformal coating on ceramic surfaces
  • Conformal coating on glass-filled epoxy surfaces
Product Family

DYMAX 984-LVF

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Single Component/Colorless Fluorescing Liquid
Specific Gravity
1.05
Physical Properties
Viscosity
150 mPa.s
Mechanical Properties
Elongation
5 %
Chemical Properties
Water Absorption
0.4 %
Other Properties
Storage Temperature
10 - 35 °C

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied characteristics used for material and process evaluation. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Solids content 100 % As supplied
Component count One-part - As supplied
Primary cure UV light - Directly exposed coating
Secondary cure Heat - Shadowed areas
Inspection response Fluorescent - Applied or cured coating under inspection light