DYMAX 9422-T-SC

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DYMAX 9422-T-SC

Main features

  • Visual See-Cure Confirmation
  • Thixotropic Edge-Dispense Control
  • Targeted Component Shock Absorption

Product Description

Dymax 9422-T-SC See-Cure Light-Cure Reinforcement Adhesive is a one-part, thixotropic reinforcement adhesive for fine-pitch and leadless components on printed circuit boards. The material cures with UV or visible light and uses See-Cure color change, shifting from blue to clear as cure develops. Its controlled-flow gel is suited to localized placement around component edges, helping the adhesive remain where reinforcement is needed before exposure. After cure, the material provides targeted component support and shock absorption without functioning as a full-area underfill.

Key features

  • Blue-to-Clear Cure Indication: See-Cure color change provides a visible cue as light cure develops.
  • Thixotropic Edge Placement: Controlled flow supports localized dispensing around component edges.
  • Targeted Shock Absorption: The cured adhesive reinforces fine-pitch and leadless PCB components.

Applications / Suitable for

  • Fine-pitch component reinforcement
  • Leadless component reinforcement
  • Localized shock absorption
Product Family

DYMAX 9422-T-SC

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Blue Transparent Liquid
Chemistry Type
Acrylated Urethane
Density (g)
1.01 g/cm3
Refractive index
1.50
Physical Properties
Viscosity
8,000 mPa.s
Mechanical Properties
Elongation
170 %
Chemical Properties
Water Absorption
4.7 %
Other Properties
Storage Temperature
10 - 35 °C

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied characteristics used for material and process evaluation. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Component count One-part - As supplied
Uncured appearance Blue gel - As supplied
Rheology Thixotropic - Controlled edge placement
Cure mechanism UV/visible light - After placement
Cure indicator See-Cure blue-to-clear response - During cure
Technical properties

After-processing / final-state properties

Final-state characteristics after the stated cure or processing condition. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Cured appearance Clear - After sufficient light cure
Cure indication Blue-to-clear transition - During cure
Reinforcement behavior Localized edge support - Fine-pitch and leadless components
Impact response Shock absorption - Reinforced PCB assembly

Leading Brands Trust in Our Products and Services