DYMAX 9422-SC

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DYMAX 9422-SC

Main features

  • See-Cure Visual Progress Check
  • High-Thixotropy Placement Control
  • Localized Shock-Absorbing Reinforcement

Product Description

Dymax 9422-SC See-Cure Light-Cure Reinforcement Adhesive is a one-part, highly thixotropic adhesive for PCB component reinforcement and bonding. UV or visible light initiates cure after placement, and the See-Cure response changes the material from blue to clear as cure develops. The non-flowing gel supports precise placement around fine-pitch and leadless components, where it adds localized reinforcement and absorbs mechanical shock. This combination gives assemblers a visible cure cue, stable dispense placement, and focused support around selected components.

Key features

  • See-Cure Visual Response: The blue-to-clear change gives a visible indication of cure progress.
  • High-Thixotropy Placement: The gel resists movement after localized dispensing around components.
  • Reinforcement and Bonding: The cured adhesive supports component reinforcement, shock absorption, and bonding.

Applications / Suitable for

  • Fine-pitch component reinforcement
  • Leadless component reinforcement
  • Localized shock absorption
  • PCB component bonding
Product Family

DYMAX 9422-SC

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Blue Transparent Gel
Chemistry Type
Acrylated Urethane
Density (g)
1.01 g/cm3
Refractive index
1.50
Physical Properties
Viscosity
38,000 mPa.s
Mechanical Properties
Elongation
170 %
Chemical Properties
Water Absorption
4.7 %
Other Properties
Storage Temperature
10 - 25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied characteristics used for material and process evaluation. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Component count One-part - As supplied
Uncured appearance Blue gel - As supplied
Rheology Highly thixotropic - Localized dispensing
Cure mechanism UV/visible light - After placement
Cure indicator See-Cure blue-to-clear response - During cure
Application behavior Controlled localized placement - Around PCB components
Technical properties

After-processing / final-state properties

Final-state characteristics after the stated cure or processing condition. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Cured appearance Clear - After sufficient light cure
Cure indication Blue-to-clear transition - During cure
Reinforcement behavior Localized component support - Cured adhesive around PCB components
Impact response Shock absorption - Reinforced component assembly
Bonding capability Component bonding - Cured adhesive

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers