DYMAX 9309-SC

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DYMAX 9309-SC

Main features

  • Blue-to-Clear Cure Confirmation
  • Thixotropic Needle or Jet Dispensing
  • Localized BGA/CSP Ruggedization

Product Description

Dymax 9309-SC See-Cure Light-Cure BGA/CSP Reinforcement Adhesive is a single-component light-curable adhesive for reinforcing BGA, CSP, fine-pitch, and leadless components on printed circuit boards. Its highly thixotropic blue gel remains positioned during needle or jet dispensing, then changes from blue to clear as cure progresses. UV or visible light produces a tack-free cured surface for localized edge bonding and component ruggedization. The material supports shock attenuation and can replace full-area underfill in selected reinforcement designs that call for targeted coverage.

Key features

  • See-Cure Color Confirmation: A blue-to-clear response helps identify sufficient light exposure.
  • Thixotropic Dispense Control: The high-viscosity gel shows minimal movement after needle or jet dispensing.
  • Localized Component Ruggedization: Edge reinforcement supports shock attenuation around BGA, CSP, and leadless packages.

Applications / Suitable for

  • BGA and CSP reinforcement
  • Fine-pitch and leadless component reinforcement
  • Localized shock attenuation
  • Targeted underfill-alternative reinforcement
Product Family

DYMAX 9309-SC

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Blue Transparent Gel
Chemistry Type
Acrylated Urethane
Density (g)
1.05 g/cm3
Refractive index
1.50
Physical Properties
Viscosity
45,000 mPa.s
Mechanical Properties
Elongation
140 %
Chemical Properties
Water Absorption
3.0 %
Other Properties
Storage Temperature
10 - 35 °C

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied characteristics used for material and process evaluation. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Chemical class Acrylated urethane - As supplied
Component count One-part - As supplied
Uncured appearance Blue transparent gel - As supplied
Viscosity 45,000 nominal cP Typical; as supplied
Rheology Highly thixotropic - Minimal movement after dispense
Solvent content No solvents added - As supplied
Dispense methods Needle or jet - Localized application
Technical properties

After-processing / final-state properties

Final-state characteristics after the stated cure or processing condition. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Cure-indicator change Blue to clear - After sufficient UV/visible-light cure
Cured appearance Clear - After cure
Surface condition Tack-free - After light cure
Reinforcement behavior Shock attenuation and ruggedization - Localized edge reinforcement

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers