DYMAX 912-A

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DYMAX 912-A

Main features

  • Quick UV Wire Tacking
  • Solvent-Free One-Part Processing
  • Localized Wire Retention

Product Description

Dymax Light Weld 912-A Adhesive for Wire Tacking is a single-component, solvent-free aerobic acrylic adhesive for wire tacking in electronics assembly. The urethane oligomer/(meth)acrylate formulation cures with UV light after routed wires are positioned. Its one-part format avoids component mixing, and the quick cure supports short, localized bonding steps. The adhesive creates focused wire retention while leaving the surrounding board area accessible, making it suited to production processes that require precise tacking rather than broad-area bonding.

Key features

  • Solvent-Free One-Part Processing: Ready-to-use format avoids component mixing and added solvent.
  • Quick UV Cure: UV activation supports short tacking cycles after wire placement.
  • Focused Wire Retention: The adhesive is formulated for localized wire-tacking tasks in electronics assembly.

Applications / Suitable for

  • Wire tacking in electronics assembly
Product Family

DYMAX 912-A

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear/Straw Liquid
Chemistry Type
Urethane Oligomer/(Meth)Acrylate Monomer Blends
Refractive index
1.48
Thermal Properties
Flash Point
>93 °C
Physical Properties
Viscosity
Thixotropic Gel mPa.s
Mechanical Properties
Elongation
12 %
Chemical Properties
Water Absorption
0.5 %
Other Properties
Storage Temperature
10 - 35 °C

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied characteristics used for material and process evaluation. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Chemical family Urethane oligomer/(meth)acrylate - As supplied
Formulation type Aerobic acrylic - As supplied
Component count One-part - As supplied
Solvent content Solvent-free - As supplied
Cure mechanism UV light - After wire placement
Cure response Quick cure - Localized wire-tacking application