DYMAX 9037-F

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DYMAX 9037-F

Main features

  • Dual Light and Heat Cure
  • Thixotropic Glob-Top Control
  • Blue-Fluorescent Coverage Inspection

Product Description

Dymax Multi-Cure 9037-F Blue Fluorescing Encapsulant/Wire Bond Adhesive is a single-component acrylated urethane encapsulant and wire-bond adhesive for chip-on-board, chip-on-flex, chip-on-glass, and wire-bond assemblies. UV or visible light provides the primary cure, while a secondary heat-cure route addresses material in shadowed areas. Its thixotropic, high-viscosity form supports controlled glob-top placement, and blue fluorescence improves visual confirmation of coverage. The cured material is clear and flexible, with moisture and thermal resistance for protected electronic components and interconnects.

Key features

  • Shadow-Area Cure Coverage: Secondary heat cure complements UV or visible light where direct exposure is limited.
  • Controlled Glob-Top Placement: Thixotropic, high-viscosity rheology retains material over chips and wire bonds.
  • Blue-Fluorescent Inspection: Fluorescence under black light supports coverage checks after dispensing.

Applications / Suitable for

  • Chip-on-board encapsulation
  • Chip-on-flex encapsulation
  • Chip-on-glass encapsulation
  • Wire bonding
Product Family

DYMAX 9037-F

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Translucent Gel
Chemistry Type
Acrylated Urethane
Density (g)
1.06 g/cm3
Refractive index
1.5
Physical Properties
Viscosity
55,000 mPa.s
Mechanical Properties
Elongation
110 %
Electrical Properties
Volume Resistivity
2.59E+10 Ohms⋅cm
Chemical Properties
Water Absorption
0.9 %
Thermal Properties
Glass Transition Temperature (Tg)
31 °C
Other Properties
Storage Temperature
10 -32 °C

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied characteristics used for material and process evaluation. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Chemical class Acrylated urethane - As supplied
Component count One-part - As supplied
Appearance Translucent gel - As supplied
Rheology Thixotropic, high viscosity - As supplied
Viscosity 55,000 nominal cP Typical; as supplied
Solvent content No solvents added - As supplied
Cure routes UV/visible light and secondary heat - Secondary heat for shadowed areas
Technical properties

After-processing / final-state properties

Final-state characteristics after the stated cure or processing condition. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Cured appearance Clear - After cure
Inspection response Blue fluorescence - Under black light
Flexibility Flexible - Cured material
Moisture resistance Resistant - Cured material; qualitative
Thermal resistance Resistant - Cured material; qualitative

Leading Brands Trust in Our Products and Services