DYMAX 9001-E-V3.5

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DYMAX 9001-E-V3.5

Main features

  • Fast Light Cure with Heat Backup
  • Clear Resilient Electronics Protection
  • Moisture and Thermal-Cycle Resistance

Product Description

Dymax Multi-Cure 9001-E-V3.5 Resilient Clear Encapsulant is a clear acrylated-urethane electronics encapsulant that cures with UV/visible light and provides secondary heat cure for shadowed areas. The nominal 17,000 cP liquid contains no nonreactive solvents and supports rapid fixture with specified Dymax curing systems; full cure depends on intensity, thickness, geometry, and substrate transmission. After UV cure followed by 15 days at 25 deg C and 50% relative humidity, it provides D45 hardness, 129% elongation, and controlled electrical properties. Applications include chip-on-board, chip-on-flex, and multi-chip module encapsulation.

Key features

  • Clear solvent-free liquid: The acrylated-urethane formulation contains no nonreactive solvents and remains clear for encapsulation.
  • Fast light cure with heat backup: UV/visible light provides primary cure, while heat can cure shadowed areas after light exposure.
  • Resilient electronics protection: The cured material combines flexibility with documented moisture and thermal-cycle resistance.

Applications / Suitable for

  • Chip-on-board encapsulation
  • Chip-on-flex encapsulation
  • Multi-chip module encapsulation
Product Family

DYMAX 9001-E-V3.5

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear Liquid
Chemistry Type
Acrylated Urethane
Density (g)
1.06 g/cm3
Refractive index
1.5
Physical Properties
Viscosity
17,000 mPa.s
Mechanical Properties
Elongation
129 %
Electrical Properties
Dielectric Strength
200 kV/mm
Volume Resistivity
555x10E12 Ohms⋅cm
Chemical Properties
Water Absorption
2.6 %
Thermal Properties
Glass Transition Temperature (Tg)
37 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured values.

Property Value Unit Method / condition
Chemical class Acrylated urethane As supplied
Appearance Clear liquid As supplied
Nonreactive solvent content None As supplied
Density 1.06 g/mL ASTM D1875
Viscosity 17,000 nominal cP ASTM D2556
Shelf life 12 months Stored at 10 to 25 deg C in the original unopened container
Technical properties

After-processing / final-state properties

Typical values after UV cure followed by 15 days at 25 deg C and 50% relative humidity.

Property Value Unit Method / condition
Durometer hardness D45 Shore D ASTM D2240
Tensile strength at break 6.9 MPa ASTM D638
Elongation at break 129 % ASTM D638
Modulus of elasticity 48.3 MPa ASTM D638
Dielectric constant 3.27 At 1 MHz; ASTM D1304
Water absorption 0.9 % 25 deg C for 24 h; ASTM D570
Glass transition temperature 37 deg C ASTM D5418