DYMAX 9-984-LVF

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DYMAX 9-984-LVF

Main features

  • Rapid UV cure
  • Bright fluorescent inspection
  • Strong substrate adhesion

Product Description

Dymax 9-984-LVF is a single-component, 100% solids UV-curable conformal coating formulated for electronic circuit board protection. Designed for rapid room-temperature cure under long-wave UV light (320-380 nm), thin coating layers cure within seconds while producing bright fluorescence for inspection under black light. The coating provides excellent adhesion to metals, ceramics, and glass-filled epoxy substrates and offers secondary heat-curing capability for shadowed areas on densely populated circuit boards. With RoHS 2015/863/EU compliance, low viscosity, durable cured properties, and long-lasting fluorescence, 9-984-LVF is suitable for electronics manufacturing environments requiring efficient coating application and cure verification.

Key features

  • Rapid UV cure: Thin coating layers cure in seconds when exposed to appropriate UV light intensity.
  • Bright fluorescent inspection: Retains high-brilliance fluorescence after curing to support black-light inspection processes.
  • Strong substrate adhesion: Exhibits excellent adhesion to metal, ceramic, and glass-filled epoxy surfaces.

Applications / Suitable for

  • Conformal coating of electronic circuit boards
  • Electronics manufacturing and assembly operations
  • UV-cured protective coatings requiring fluorescent inspection
  • Densely populated circuit boards requiring secondary heat cure in shadowed areas
Product Family

DYMAX 9-984-LVF

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Single Component/Clear Fluorescing Liquid
Specific Gravity
1.05
Physical Properties
Viscosity
150 mPa.s
Mechanical Properties
Elongation
5 %
Chemical Properties
Water Absorption
0.4 %
Other Properties
Storage Temperature
10 - 32 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured properties of Dymax 9-984-LVF prior to UV curing.

Property Value Unit Method / condition
Solvent Content None - Typical uncured property
Appearance Clear fluorescing liquid - Single-component material
Specific Gravity 1.05 - Typical uncured property
Viscosity 150 cP Nominal, ASTM D-1384
Shelf Life 18 months 10°C to 32°C, unopened container
Technical properties

After-processing / final-state properties

Typical cured properties after UV curing.

Property Value Unit Method / condition
Durometer Hardness D80 Shore D ASTM D-224
Tensile Strength at Break 6000 psi ASTM D-638
Elongation at Break 5 % ASTM D-638
Dielectric Strength 1800 V/mil ASTM D-1304
Dielectric Constant 3.4 - 1 MHz, ASTM D-1304