DYMAX 9-911-REV-A

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DYMAX 9-911-REV-A

Main features

  • Dual-cure capability
  • High-viscosity gel formulation
  • Fast processing

Product Description

Dymax Multi-Cure® 9-911-REV-A is a light-curable wire-tacking adhesive formulated for printed circuit board repair, jumper-wire bonding, and wire stabilization applications. This acrylated urethane adhesive cures rapidly upon exposure to UV and visible light and incorporates a secondary heat-cure capability for shadowed areas where light exposure is limited. Its high-viscosity gel consistency helps maintain wire placement and coverage during assembly and repair processes. The material is solvent-free, blue fluorescing for visual inspection, and compatible with Dymax conformal coating systems used in electronic assembly environments.

Key features

  • Dual-cure capability: UV/visible light cure combined with secondary heat cure supports processing in shadowed areas.
  • High-viscosity gel formulation: Nominal viscosity of 36,000 cP helps maintain wire position and provides controlled coverage during PCB repair.
  • Fast processing: Achieves fixture times as low as 1 second under appropriate Dymax curing systems.

Applications / Suitable for

  • Wire tacking on printed circuit boards
  • Bonding jumper wires
  • PCB repair operations
  • Electronic assembly applications requiring UV/visible light curing
  • Applications with limited light access using secondary heat cure
Product Family

DYMAX 9-911-REV-A

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear Translucent Gel
Chemistry Type
Acrylated Urethane
Density (g)
1.07 g/cm3
Physical Properties
Viscosity
36,000 mPa.s
Mechanical Properties
Elongation
18 %
Chemical Properties
Water Absorption
1.2 %
Other Properties
Storage Temperature
10 - 32 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Representative uncured properties for Dymax Multi-Cure® 9-911-REV-A.

Property Value Unit Method / condition
Chemical Class Acrylated Urethane - Uncured material
Appearance Clear Translucent Gel - As supplied
Density 1.07 g/mL ASTM D1875
Viscosity 36,000 (nominal) cP ASTM D2556, 20 rpm
Solvent Content No Nonreactive Solvents - Supplier reported
Technical properties

After-processing / final-state properties

Representative cured mechanical properties.

Property Value Unit Method / condition
Durometer Hardness D80 Shore D ASTM D2240
Tensile Strength at Break 28 MPa ASTM D638
Elongation at Break 18 % ASTM D638
Modulus of Elasticity 690 MPa ASTM D638