DYMAX 9-7001

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DYMAX 9-7001

Main features

  • Thixotropic Pink Dispense Control
  • Wave-Solder and Reflow Protection
  • One-Piece Residue-Free Removal

Product Description

Dymax SpeedMask 9-7001 PCB Protective Maskant is a single-component pink peelable maskant for temporary PCB protection during solvent-based conformal coating, wave soldering, and reflow. Its thixotropic acrylated urethane gel supports controlled manual or automated dispensing and remains visible against common board surfaces. UV or visible light converts the applied material into a removable process barrier. The cured mask tolerates the intended assembly exposure, then peels away in one piece without residue when used within the prescribed process, including protection around gold- and copper-plated pins.

Key features

  • Pink Thixotropic Placement: High visual contrast and controlled flow support accurate dispensing.
  • Multi-Process PCB Protection: The cured barrier protects selected areas during conformal coating, wave soldering, and reflow.
  • One-Piece Clean Removal: The mask peels away after processing without residue under the stated process.

Applications / Suitable for

  • PCB masking during solvent-based conformal coating
  • PCB masking during wave soldering
  • PCB masking during reflow
Product Family

DYMAX 9-7001

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Pink Translucent Gel in Uncured State
Chemistry Type
Acrylated Urethane
Density (g)
1.14 g/cm3
Physical Properties
Viscosity
40,000 mPa.s
Mechanical Properties
Elongation
180 %
Chemical Properties
Water Absorption
16.6 %
Other Properties
Storage Temperature
10 - 32 °C

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied characteristics used for material and process evaluation. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Chemical class Acrylated urethane - As supplied
Component count One-part - As supplied
Uncured appearance Pink translucent gel - As supplied
Rheology Thixotropic - Manual or automated dispensing
Halogen content Halogen-free - As supplied
Silicone content Silicone-free - As supplied
Cure mechanism UV/visible light - After application
Technical properties

After-processing / final-state properties

Final-state characteristics after the stated cure or processing condition. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Final form Peelable protective mask - After light cure
Removal behavior Peels in one piece - After PCB processing
Residue after removal None - Properly cured and removed
Thermal process exposure Wave solder and reflow - Cured mask
Coating compatibility Solvent-based conformal coating barrier - Cured mask
Protected finishes Gold- and copper-plated pins - Temporary masking

Leading Brands Trust in Our Products and Services