DYMAX 9-20557

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DYMAX 9-20557

Main features

  • Flexible Low-Modulus Protection
  • Light and Shadow-Area Cure
  • Fluorescent Conformal-Coverage Inspection

Product Description

Dymax Multi-Cure 9-20557 Flexible Light-Cure Conformal Coating is a single-component, medium-viscosity conformal coating for printed circuit boards and electronic assemblies. UV or visible light cures exposed areas, while secondary heat cure develops coating in shadowed regions. The flexible, low-modulus cured film provides protective coverage without the rigidity of a bulk encapsulant. Blue fluorescence supports inspection, and the coating can be applied across metal, ceramic, PCB, flex, and silicon surfaces. Its solvent-free acrylated urethane form avoids component mixing and supports controlled dispensing.

Key features

  • Flexible Low-Modulus Protection: The cured film combines conformal coverage with a flexible mechanical profile.
  • Light Plus Shadow-Area Cure: UV or visible light cure is complemented by secondary heat cure in shaded regions.
  • Blue-Fluorescent Inspection: Fluorescence under black light supports coating coverage checks.

Applications / Suitable for

  • Conformal coating of printed circuit boards
  • Conformal coating of electronic assemblies
Product Family

DYMAX 9-20557

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear to Light Yellow
Chemistry Type
Acrylated Urethane
Refractive index
1.51
Physical Properties
Viscosity
2,300 mPa.s
Mechanical Properties
Elongation
110 %
Chemical Properties
Water Absorption
1.0 %
Other Properties
Storage Temperature
10 - 32 °C

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied characteristics used for material and process evaluation. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Solvent content No nonreactive solvents - As supplied
Chemical class Acrylated urethane - As supplied
Appearance Clear to light yellow - As supplied
Density 1.05 g/ml ASTM D1875
Viscosity 2,300 nominal cP ASTM D1084; 20 rpm
Shelf life 12 months Original unopened container; store at 10 to 32 deg C
Technical properties

After-processing / final-state properties

Final-state characteristics after the stated cure or processing condition. Numerical values are typical unless otherwise identified.

Property Value Unit Method / condition
Durometer hardness D60 - ASTM D2240
Tensile strength at break 10 (1,500) MPa (psi) ASTM D638
Elongation at break 110 % ASTM D638
Modulus of elasticity 89 (13,000) MPa (psi) ASTM D638
Boiling water absorption 2.7 % ASTM D570; 2 hr
Water absorption 1.0 % ASTM D570; 25 deg C for 24 hr
Dielectric withstand voltage >1,500 V MIL-I-46058C
Volume resistivity 1.48 x 10^15 ohm cm ASTM D257