Main features

  • Light Cure with Heat Backup
  • Aggressive Acid-Process Protection
  • Peel or Incineration Removal

Product Description

Dymax SpeedMask 758-H Maskant is a red opaque gel maskant for acid stripping, plating-bath exposure, and aggressive grit blasting on titanium and nickel alloys. The material cures with LED or UV/visible light and includes secondary heat cure for internal passages or other shadowed areas that are difficult to expose directly. Its application behavior supports spraying and trimming before or during process preparation. After the protected operation, the mask can be removed by peeling or incineration within the stated chemical, geometry, and cure conditions.

Key features

  • Light cure with heat backup: LED or UV/visible exposure provides primary cure, with secondary heat cure for internal passages.
  • Acid-process resistance: The cured mask is documented for acid stripping and plating-bath protection.
  • Adaptable removal: The temporary barrier supports peel or incineration removal after processing.

Applications / Suitable for

  • Acid stripping
  • Plating-bath protection
  • Aggressive grit blasting on titanium and nickel alloys
Product Family

DYMAX 758-H

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Red Opaque Gel
Density (g)
1.08 g/cm3
Mechanical Properties
Elongation
140 %
Chemical Properties
Water Absorption
0.5 %
Physical Properties
Viscosity
11,500 mPa.s
Other Properties
Storage Temperature
10 - 32 °C
Thermal Properties
Glass Transition Temperature (Tg)
26 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Product characteristics before and during light or secondary heat cure.

Property Value Unit Method / condition
Physical form Opaque gel maskant As supplied
Color Red Before cure
Primary cure activation LED or UV and visible light Applied maskant
Secondary cure Heat Internal passages or shadowed areas
Application behavior Sprayable and trimmable During mask preparation
Technical properties

After-processing / final-state properties

Cured-mask behavior within the stated acid-processing and removal conditions.

Property Value Unit Method / condition
Chemical process scope Acid stripping; plating baths Stated operations
Acid resistance Aggressive chemical-process protection Within stated exposure limits
Mechanical process scope Aggressive grit blasting Titanium and nickel alloy applications
Removal methods Peel; incineration After processing
Final application boundary Temporary removable mask Not a permanent coating