DYMAX 750-SC

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

DYMAX 750-SC

Main features

  • Visual See-Cure Color Change
  • Sprayable Thermal-Spray Coverage
  • Hard High-Adhesion Protection

Product Description

Dymax SpeedMask 750-SC Maskant is a See-Cure UV/visible-light-curable process maskant that changes from purple to pink as cure develops. Its sprayable gel behavior supports controlled coverage for high-temperature plasma spray, HVOF, wire arc, thermal-spray coating, and aggressive grit-blasting operations. After cure, the mask is stated as high adhesion, hard, and durable for temporary process protection. The product is also listed for orthopedic implant protection with ISO 10993-5 cytotoxicity evaluation scope, which must remain tied to the exact stated conditions.

Key features

  • Purple-to-pink cure indication: The See-Cure color change provides a visual cue as light cure develops.
  • Sprayable gel coverage: The material supports controlled application over thermal-spray masking areas.
  • Hard durable barrier: The cured mask provides high adhesion for aggressive thermal and abrasive processing.

Applications / Suitable for

  • High-temperature plasma spray and HVOF
  • Wire arc and thermal-spray coating
  • Aggressive grit blasting and orthopedic implant process protection
Product Family

DYMAX 750-SC

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Translucent Purple Gel
Density (g)
1.06 g/cm3
Mechanical Properties
Elongation
140 %
Chemical Properties
Water Absorption
0.6 %
Physical Properties
Viscosity
30,000 mPa.s
Other Properties
Storage Temperature
10 - 35 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Product characteristics before and during light cure.

Property Value Unit Method / condition
Physical form Sprayable gel maskant As supplied
Uncured color Purple Before light exposure
Cure activation UV and visible light Applied maskant
Cure indicator Purple-to-pink color change During light cure
Process role Temporary thermal-spray protection Before the Stated operations
Technical properties

After-processing / final-state properties

Cured-mask characteristics Within the stated process and evaluation scope.

Property Value Unit Method / condition
Cured color Pink After sufficient light exposure
Cured adhesion High During the protected process
Cured character Hard and durable After light cure
Biological evaluation scope ISO 10993-5 cytotoxicity evaluation Within the stated test scope
Final application boundary Temporary removable mask Not a permanent coating