DYMAX 750

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

DYMAX 750

Main features

  • High-Temperature Thermal-Spray Masking
  • Aggressive Blast-Media Resilience
  • Flexible Post-Process Removal

Product Description

Dymax SpeedMask 750 Maskant is a pink UV/visible-light-curable gel maskant for temporary protection during high-temperature thermal-spray coating and aggressive grit-blasting operations. The material supports high adhesion and tack-free cure, helping the mask remain in place while exposed to plasma spray, HVOF, wire arc, and related blast-media conditions. Supported substrates include nickel, titanium, and cobalt-chrome alloys. After processing, the cured mask can be removed by incineration or by warm-water and air-assisted methods within the stated process conditions.

Key features

  • Pink gel coverage: The colored gel supports controlled placement on selected alloy surfaces before cure.
  • Thermal-spray resilience: The cured mask is documented for high-temperature spray and aggressive blast-media exposure.
  • Multiple removal routes: Post-process removal can use incineration or warm-water and air-assisted methods.

Applications / Suitable for

  • High-temperature plasma spray and HVOF
  • Wire arc and thermal-spray coating
  • Aggressive grit blasting on nickel, titanium, and cobalt-chrome alloys
Product Family

DYMAX 750

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Translucent Pink Gel
Density (g)
1.06 g/cm3
Mechanical Properties
Elongation
140 %
Chemical Properties
Water Absorption
0.5 %
Physical Properties
Viscosity
30,000 mPa.s
Other Properties
Storage Temperature
10 - 32 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Product characteristics before thermal-spray or blast-media exposure.

Property Value Unit Method / condition
Physical form Gel maskant As supplied
Color Pink Before cure
Cure activation UV and visible light Applied maskant
Cure response High adhesion with tack-free behavior After sufficient light exposure
Process role Temporary high-temperature masking Before thermal spray or grit blasting
Technical properties

After-processing / final-state properties

Cured-mask behavior within stated thermal-spray, blasting, and removal conditions.

Property Value Unit Method / condition
Process-temperature role High-temperature process masking During supported thermal-spray operations
Blast-media behavior Resilient under aggressive grit blasting Within stated conditions
Alloy scope Nickel; titanium; cobalt-chrome Substrate scope
Removal methods Incineration; warm water with air assistance After processing
Final application boundary Temporary removable mask Not a permanent coating