DYMAX 728-G

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

DYMAX 728-G

Main features

  • High-Visibility Process Masking
  • High-Adhesion Aggressive-Process Protection
  • Removable Post-Process Barrier

Product Description

Dymax SpeedMask 728-G Maskant is a high-visibility green UV/visible-light-curable process maskant for temporary surface protection during plating, anodizing, aggressive grit blasting, shot peening, and machining. Its gel form supports controlled placement on selected areas before exposure, while the cured mask provides high adhesion through demanding processing and remains removable after the operation. The product is also stated for orthopedic implant protection, with cytotoxicity evaluation under ISO 10993-5. It functions as a removable process barrier rather than a permanent surface coating.

Key features

  • High-visibility green placement: The green gel supports visual confirmation of mask coverage before cure.
  • Aggressive-process retention: High cured adhesion supports temporary protection through blasting, peening, plating, and machining.
  • Removable protective barrier: The cured mask is intended for post-process removal instead of permanent surface protection.

Applications / Suitable for

  • Plating and anodizing
  • Aggressive grit blasting, shot peening, and machining
  • Orthopedic implant process protection within the documented scope
Product Family

DYMAX 728-G

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Green/Blue Translucent Gel
Density (g)
1.02 g/cm3
Mechanical Properties
Elongation
265 %
Chemical Properties
Water Absorption
2.3 %
Physical Properties
Viscosity
25,000 mPa.s
Other Properties
Storage Temperature
10 - 32 °C
Thermal Properties
Glass Transition Temperature (Tg)
43 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Product characteristics before process exposure and final mask removal.

Property Value Unit Method / condition
Physical form Green gel maskant As supplied
Placement visibility High-visibility green Before cure
Cure activation UV and visible light Applied maskant
Application behavior Localized gel placement Before cure
Process role Temporary surface protection Before plating, blasting, peening, or machining
Technical properties

After-processing / final-state properties

Cured-mask characteristics Within the stated processing and evaluation scope.

Property Value Unit Method / condition
Cured adhesion High During the protected process
Mechanical process scope Aggressive grit blasting; shot peening; machining Stated operations
Electrochemical process scope Plating; anodizing Stated operations
Biological evaluation scope ISO 10993-5 cytotoxicity evaluation Within the stated test scope
Final application boundary Temporary removable mask Not a permanent coating