DYMAX 726-SC

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

DYMAX 726-SC

Main features

  • Visual See-Cure Verification
  • Flexible Multi-Process Protection
  • OMat and ISO Evaluation Scope

Product Description

Dymax SpeedMask 726-SC Maskant is a See-Cure process maskant that changes from blue before cure to pink after UV or visible light exposure. The color transition provides an immediate visual cue for cure progress while the material protects selected areas during plating, anodizing, gritting, shot peening, air plasma spray, and low-temperature powder coating. The cured mask is formulated to remain flexible across the stated process-temperature range and includes product-specific mechanical and qualification data. Its application scope also includes orthopedic implant protection where the exact ISO 10993-5 and Rolls-Royce OMat boundaries are retained.

Key features

  • Blue-to-pink cure indication: See-Cure color change gives a visible cue from uncured blue to cured pink.
  • Cross-process masking range: The material supports plating, peening, plasma spray, and low-temperature powder coating.
  • Qualified application scope: The source package includes Rolls-Royce OMat and ISO 10993-5 evaluation context.

Applications / Suitable for

  • Plating and anodizing
  • Gritting, shot peening, and air plasma spray
  • Low-temperature powder coating and orthopedic implant protection
Product Family

DYMAX 726-SC

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Blue Translucent Gel
Density (g)
1.13 g/cm3
Mechanical Properties
Elongation
160 %
Chemical Properties
Water Absorption
20 %
Physical Properties
Viscosity
52,000 mPa.s
Other Properties
Storage Temperature
10 - 32 °C
Thermal Properties
Glass Transition Temperature (Tg)
39 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Before-processing characteristics for placement and visual cure verification.

Property Value Unit Method / condition
Physical form Removable process maskant As supplied
Uncured color Blue Before light exposure
Cure activation UV and visible light Applied maskant
Cure indicator Blue-to-pink color change During light cure
Process role Temporary surface protection Before the Stated operations
Technical properties

After-processing / final-state properties

Cured-state characteristics, process scope, and product-specific evaluation boundaries.

Property Value Unit Method / condition
Cured color Pink After sufficient light exposure
Mechanical data scope Shore D hardness and cured modulus Product-specific cured-material evaluation
Process-temperature behavior Flexible within the stated range During supported processing
Qualification scope Rolls-Royce OMat Exact product scope
Biological evaluation scope ISO 10993-5 cytotoxicity evaluation Within the stated test scope