DYMAX 718

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

DYMAX 718

Main features

  • Multi-Process Thermal-Spray Masking
  • Opaque Gel Coverage Control
  • Defined Incineration Removal

Product Description

Dymax SpeedMask 718 Maskant is an opaque gel maskant for temporary protection during thermal-spray coating processes. The material is used with air plasma spray, HVOF, wire arc spray, and D-Gun coating operations where the applied mask must resist the process and preserve selected component areas. Light cure converts the placed gel into a durable temporary barrier, and the stated removal route uses incineration after processing. The product is used specifically for thermal-spray masking rather than general-purpose coating. Its application value comes from gel placement, cured process resistance, and a defined post-process removal method across several spray technologies.

Key features

  • Thermal-spray process coverage: The maskant supports air plasma, HVOF, wire arc, and D-Gun coating operations.
  • Opaque gel placement: The gel form supports localized application and visible coverage before cure.
  • Incineration removal route: The cured mask is removed by the documented burn-off process after coating.

Applications / Suitable for

  • Air plasma spray
  • HVOF and wire arc spray
  • D-Gun coating
Product Family

DYMAX 718

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Opaque Gel
Density (g)
1.70 g/cm3
Mechanical Properties
Elongation
3 %
Chemical Properties
Water Absorption
2.7 %
Physical Properties
Viscosity
46,000 mPa.s
Other Properties
Storage Temperature
10 - 32 °C

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied and pre-cure characteristics.

Property Value Unit Method / condition
Physical form Opaque gel As supplied
Application behavior Localized mask placement Before cure
Cure activation UV and visible light Applied maskant
Primary function Thermal-spray process masking Before coating exposure
Supported spray processes Air plasma; HVOF; wire arc; D-Gun Application scope
Technical properties

After-processing / final-state properties

Final cured-mask characteristics during thermal-spray exposure and removal.

Property Value Unit Method / condition
Cured function Temporary thermal-spray barrier After light cure
Process resistance Thermal-spray exposure Within the stated spray processes
Removal method Incineration After coating
Protected operations Air plasma; HVOF; wire arc; D-Gun coating Stated operations
Final application boundary Temporary removable mask Not a permanent coating