DYMAX 717-R

Main features

  • High-Adhesion Process Retention
  • Hot-Water-Assisted Peel Removal
  • Visible Red Mask Placement

Product Description

Dymax SpeedMask 717-R Maskant is a red UV- and visible-light-curable gel maskant for plating, anodizing, aggressive grit blasting, shot peening, machining, and air plasma spray. The product provides high adhesion during process exposure and is removed with a hot-water-assisted peel sequence after use. Its supported application scope also includes protection of orthopedic implants where the exact process and biological-evaluation boundaries are maintained. The gel form supports controlled placement before cure, while the red appearance improves visual identification of masked areas. SpeedMask 717-R is a temporary process-protection material and is not intended to remain as a permanent coating.

Key features

  • Red visual identification: The red gel makes the applied mask area easy to distinguish before and after cure.
  • High-adhesion process hold: The cured mask is intended to remain attached through plating and aggressive mechanical processing.
  • Hot-water-assisted release: The documented removal sequence combines hot water with peel removal after processing.

Applications / Suitable for

  • Plating and anodizing
  • Aggressive grit blasting, shot peening, and machining
  • Air plasma spray and orthopedic implant protection
Product Family

DYMAX 717-R

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Red Translucent Gel
Density (g)
1.10 g/cm3
Mechanical Properties
Elongation
210 %
Chemical Properties
Water Absorption
2.6 %
Physical Properties
Viscosity
23,500 mPa.s
Other Properties
Storage Temperature
10 - 32 °C

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied characteristics for placement, identification, and light cure.

Property Value Unit Method / condition
Physical form Gel maskant As supplied
Color Red Before cure
Cure activation UV and visible light Applied maskant
Placement behavior Localized gel application Before cure
Process role Temporary surface protection Before plating, blasting, machining, or spray exposure
Technical properties

After-processing / final-state properties

Cured-mask characteristics, removal, and stated evaluation scope.

Property Value Unit Method / condition
Cured adhesion High During the protected process
Removal method Hot-water-assisted peel After processing
Process exposure scope Plating; anodizing; blasting; peening; machining; plasma spray Stated operations
Biological evaluation scope ISO 10993-5 cytotoxicity evaluation Within the stated test scope
Final application boundary Temporary removable mask Not a permanent coating